Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 장력법을 적용한 박판블록의 변형제어에 관한 연구A Study on the Deformation Control of Thin Plate Block by Applying the Tensioning Method

Journal of KWJS 2007;25(5):59-63.
Published online January 28, 2008.
장력법을 적용한 박판블록의 변형제어에 관한 연구A Study on the Deformation Control of Thin Plate Block by Applying the Tensioning Method
, ,
 
장력법을 적용한 박판블록의 변형제어에 관한 연구A Study on the Deformation Control of Thin Plate Block by Applying the Tensioning Method
Cheol-Ho Kim, Jong-Soo Yang, Ho-Kyung Kim
Abstract
  The weld-induced deformation is more serious in thin plates than in thick plates because heat affect zone of thin plates is wider than that of thick plates and in addition internal and external constraints have much more influence upon weld-induced deformation of thin plates. This paper deals with the application of the mechanical tensioning method to butt weld of thin plates to reduce the transverse and longitudinal deformation. In order to investigate the quantitative effect of tensioning method upon the reduction of angular deformation and shrinkage in longitudinal and transverse direction of weld line, butt welding test has been carried out for several thin plate specimens with varying plate thickness and magnitude of tensile load. From the present experimental study, it has been found that the tensioning method is very effective in reducing the weld-induced residual stress as well as the weld-induced deformation.
Key Words: Longitudinal shrinkage, Transverse shrinkage, Distortion, Residual Stress, Tension load, Thin plate
TOOLS
METRICS Graph View
  • 1,525 View
  • 0 Download
Related articles


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI