Previous issues
Volume 12 Issue 1
-
Porosity in Thick Aluminium Alloy Welds ( Causes and Prevention )
- 김종희, 박동환
- Journal of KWJS. 1994;12(1):7-15.
-
Gas Metal Arc Welding of Aluminum Alloys
- 윤광희, 한용섭
- Journal of KWJS. 1994;12(1):16-27.
-
Weld Cracking of High Strength Al-Zn-Mg Alloy Weldment
- 김환태, 황선효, 남수우
- Journal of KWJS. 1994;12(1):28-37.
-
Weldabilities of 7000 Aluminium Alloys ( I )
- 박성탁, 정재필, 서창제
- Journal of KWJS. 1994;12(1):38-43.
-
The Trend of Fuzzy-Controlled Welding machnines in Japan
- 박송춘, 라규환
- Journal of KWJS. 1994;12(1):44-50.
-
Effect of Shielding Gas on the MAG Welding Characteristics and Cost Reduction
- R. Killing, 황선효, 정재필, 박영조
- Journal of KWJS. 1994;12(1):51-58.
-
Control of Weld Pool Size in GMA Welding Process Using Neural Networks
- 임태균, 조형석, 부광석
- Journal of KWJS. 1994;12(1):59-72.
-
A Study of Low Cycle Fatigue Properties in CR60 , SM50Q Steel and the Weldments
- 김창주, 염태동, 조수형, 유인석, 위창욱
- Journal of KWJS. 1994;12(1):73-79.
-
Failure analyses of friction welded Al / Cu joints
- 박재현, 권영각, 장래웅
- Journal of KWJS. 1994;12(1):80-93.
-
Effects of Plasma Spray Conditions on Photoelectric Properties of Plasma Sprayed TiO2 Semiconductor
- 박정식, 박경채
- Journal of KWJS. 1994;12(1):94-101.
-
A Study on the Fatigue Strength and Allowable Stress of INVAR ( Fe-36% Ni ) Steel Lap Joint Applied to Cargo Containment of LNG Carrier
- 한명수, 한종만, 한용섭
- Journal of KWJS. 1994;12(1):102-115.