Previous issues
Volume 13 Issue 2
-
Evaluation of Material Degradation and Life Prediction for High Temperature Structures
- 정세희
- Journal of KWJS. 1995;13(2):1-11.
-
Remaining Life Assessment of High Temperature Steam Piping
- 윤기봉
- Journal of KWJS. 1995;13(2):12-24.
-
Assessment on the Crack Growth of High Temperature Header at Boiler
- 김건영, 송기욱
- Journal of KWJS. 1995;13(2):25-31.
-
A Counterplan and Life Prediction of Degradaded Structures
- 권재도, 진영준
- Journal of KWJS. 1995;13(2):32-41.
-
Development of the Advanced NDI Technique Using an Alternating Current - the Evaluation of surface crack and blind surface crack and the detection of defects in a field component -
- 김훈, 임재규
- Journal of KWJS. 1995;13(2):42-52.
-
Non-corrosive Flux Brazing of Aluminum - Brazing Technology and Trend in Japan ( 3 )
- 정재필, 죽본정, 강춘식
- Journal of KWJS. 1995;13(2):53-59.
-
The Influence of Initial Overloads on the Fatigue Life of Spot-welded Tensile-shear Specimens
- 강성수, 정원욱
- Journal of KWJS. 1995;13(2):60-67.
-
Analytical Solution for Transient Temperature Distribution in Fillet Arc Welding
- 정선국, 조형석
- Journal of KWJS. 1995;13(2):68-81.
-
Quality Improvement on Joints of Electronic Materials and Its Reliabilty by Fe-Ni Alloy Clad Lead Frame.
- 신영의, 최인수, 안승호
- Journal of KWJS. 1995;13(2):82-88.
-
Study on Wear and Corrosion Resistance of Porosity Controlled Thermal Sprayed WC Coatings
- 박정식, 양병모, 이재관, 김종철, 박경채
- Journal of KWJS. 1995;13(2):89-95.
-
A Modification in the Analysis of the Growth Rate of Short Fatigue Cracks in S45C Carbon Steel under Reversed Loading
- A.J. McEvily, 신용승
- Journal of KWJS. 1995;13(2):96-105.
-
Characteristics of Adhesive Bonded Joints of Steels for Automobile ( I )
- 윤병현, 권영각
- Journal of KWJS. 1995;13(2):106-114.
-
Modeling of Metal Transfer in GMA Welding Process
- 이강희, 최상균, 유중돈
- Journal of KWJS. 1995;13(2):115-121.
-
Effect of cooling rate on the microstructure and impact toughness of Cu-bearing HSLA steels
- 박태원, 심인옥, 김영우, 강정윤, 박화순
- Journal of KWJS. 1995;13(2):122-131.
-
Liquid Phase Diffusion Bonding Procedure of Rene80 / B / Rene80 System - Liquid Phase Diffusion Bonding Using B Powder Coating Method
- 정재필, 강춘식
- Journal of KWJS. 1995;13(2):132-138.
-
Evaluation of Underclad Crack Susceptibility of the SA508 Class 3 Steel for Pressure Vessels - Optimization of Heat Input -
- 김석원, 양성호, 김준구, 이영호
- Journal of KWJS. 1995;13(2):139-149.