Previous issues
Volume 19 Issue 6
-
Fundamentals of Fusion Welding (Ⅵ) - Fundamentals of One Sided Welding
- 정호신
- Journal of KWJS. 2001;19(6):1-6.
-
Some Aspects of Friction Stir Welding and Its Application Technologies
- 장웅성, 최기용, 김숙환, 권영각
- Journal of KWJS. 2001;19(6):7-15.
-
Microstructures and Characteristics of Friction-Stir-Welded Joints in Aluminium Alloys
- 연윤모, 이원배, 정승부
- Journal of KWJS. 2001;19(6):16-22.
-
Bonding of Magnesium Alloys by Friction Stir Welding
- 이원배, 연윤모, 서창제, 정승부
- Journal of KWJS. 2001;19(6):23-28.
-
Research Trends on the Numerical Simulation of FSW
- 방한서, 김홍주, 김영표, 장웅성
- Journal of KWJS. 2001;19(6):29-31.
-
A Study on Welded Line Detection and Wire Feeding Rate Control in GMAW with Vision Sensor
- 조택동, 김옥현, 양상민, 조만호
- Journal of KWJS. 2001;19(6):32-39.
-
Fatigue Properties of Friction Weld According to the Location of Small Artifical Defect
- 이상열, 정재강
- Journal of KWJS. 2001;19(6):40-45.
-
A Study on Hot Cracking in Ni-Base Superalloy Welds (Ⅰ) - Effect of Fe Contents on Soldification Cracking Susceptibility in Weld Metal
- 우인수, 강정윤, 西本和俊
- Journal of KWJS. 2001;19(6):46-53.
-
The Effect of Process Parameter on the Symmetry of Nugget in Micro-resistance Series Spot Welding
- 조상명, 김송미
- Journal of KWJS. 2001;19(6):54-61.
-
Characteristics of Spatter Generation in the Short Circuit Transfer Region of CO₂ Arc Welding
- 안영호, 이종봉, 최원규
- Journal of KWJS. 2001;19(6):62-67.
-
Residual Stress and Fracture Analysis of Thick Plate for Partial Penetration Multi-pass Weldment
- 김석, 심용래, 배성인, 송정일
- Journal of KWJS. 2001;19(6):68-74.
-
Development of Waveform Control for Suppressing the Spatter Generation in High Current CO₂ Welding
- 김희진, 강봉용
- Journal of KWJS. 2001;19(6):75-83.
-
A Study on the Fatigue Characteristics and the Behavior of Crack Propagation by Overload and Bending Moment in Car Body Structure
- 성기찬, 장경복, 정진우, 강성수
- Journal of KWJS. 2001;19(6):84-89.
-
A Study on the Analysis of the Thermal Stress in Process of STS 304 TIG Welding
- 고준빈, 최원두, 이영호
- Journal of KWJS. 2001;19(6):90-95.
-
A Study on the Analysis of Residual Stress of STS 304 Weldment Using Hole Drilling Method
- 고준빈, 최원두, 이영호
- Journal of KWJS. 2001;19(6):96-102.
-
Information of New Welding Technology : Digital GMAW Power Supply
- 편집부
- Journal of KWJS. 2001;19(6):103-106.