Previous issues
Volume 30 Issue 2
-
Methods for Fatigue Strength Improvement of the Weld Structure (Ⅱ) - Post Weld Improvement Methods
- Yong Kim, Bo-Young Lee
- Journal of KWJS. 2012;30(2):1-4.
-
Competency Units for National Competency Standards Development of Welding Technology
- Jin-Hyun Koh, Seong-Joo Choi
- Journal of KWJS. 2012;30(2):5-10.
-
Micro TIG Welding Characteristics of Stainless Steel Bellows
- Yong Kim, Ki-Young Park
- Journal of KWJS. 2012;30(2):11-15.
-
The Study of Measurement of Residual Stress for Pipe Weldments of Power Plant
- Sang-Ki Park, Yean-Shik Ahn, Doo-Song Gil
- Journal of KWJS. 2012;30(2):16-21.
-
Development and Application of the Battelle Structural Stress Method for Fatigue Evaluation of Welded Automotive Structures
- JeongK. Hong
- Journal of KWJS. 2012;30(2):22-30.
-
Application of Friction Stir Welding Processes for Aluminum alloy Boat
- Je-Hyoung Cho, Myung-Hyun Kim, Jun-Woong Choi
- Journal of KWJS. 2012;30(2):31-36.
-
Overview of Research Works Regarding Welding Distortion
- Sung-ku Kang, Jong-soo Yang
- Journal of KWJS. 2012;30(2):37-42.
-
Trends of Welding Deformation Analysis for Ship Structure
- JinOh. Yun, ChongIn. Oh
- Journal of KWJS. 2012;30(2):43-46.
-
Analysis of Residual Stress on Dissimilar Butt Joint by TIG Assisted Hybrid Friction Stir Welding
- Bang Hee-Seon, Ro Chan-Seoung, M.S. Bijoy, Bang Han-Sur, Lee Yoon-Ki
- Journal of KWJS. 2012;30(2):47-53.
-
Effect of Welding Condition and Roller on Weldability of Al Coated Steel Sheet using Plasma Arc Welding
- Tae-Woo Lee, Cheol-Ho Park, Namhyun Kang, Myung-Duk Kim
- Journal of KWJS. 2012;30(2):54-58.
-
A Prediction of the Penetration Depth on CO₂ Arc Welding of Steel Sheet Lap Joint with Fillet for Car Body using Multiple Regression Analysis Technique
- Kyungmin Lee, Hyunwoo Sim, Jaehyung Kwon, Bukdong Yoon, Minki Jeong, Moonsoo Park, Boyoung Lee
- Journal of KWJS. 2012;30(2):59-64.
-
Behavior of Vibration Fracture for Sn-Ag-Cu-X Solders by Soldering
- Sanghun Jin, Namhyun Kang, Kyung-mox Cho, Changwoo Lee, Wonsik Hong
- Journal of KWJS. 2012;30(2):65-69.
-
Effect of Nitrogen Volume in Ar-N2 Shielding Gas on Microstructure and Hardness of GTA Welded Pure Ti
- Hyun-Jun An, Ae-Jeong Jeon, Jae-Keun Hong, Bo-Young Jeong, Jong-Sub Lee, Chung-Yun Kang
- Journal of KWJS. 2012;30(2):70-75.
-
Hardness Distribution and Microstructures of Electric Resistance Spot Welded 1GPa Grade Dual Phase Steel
- Hye-Sung Na, Jong-Pan Kong, Tae-Kyo Han, Kwang-Geun Chin, Chung-Yun Kang
- Journal of KWJS. 2012;30(2):76-80.
-
New Papers Published in Foreign Journals
- 편집부
- Journal of KWJS. 2012;30(2):81-84.
-
Qualification of Korean Welding Engineer, 2012
- 편집부
- Journal of KWJS. 2012;30(2):85-85.
-
학회소식
- 편집부
- Journal of KWJS. 2012;30(2):86-89.
-
회원사 동정
- 편집부
- Journal of KWJS. 2012;30(2):90-94.
-
大韓熔接·接合學會誌 第30卷 第2號 목차
- 편집부
- Journal of KWJS. 2012;30(2):95-96.