Research Papers
Effect of Carburization on the Microstructure and Laser Weldability of 316L Stainless Steel
- Gitae Park, Mokyoung Lee, Chan Kyu Kim, Sangwoo Song, Sung Chul Cha, Heon Joon Park, Jun-Ho Kim, Boyoung Jeong
- J Weld Join. 2023;41(6):475-485.
-
Research Papers
T-joint Fillet Laser Welding of High-Strength Stainless Steel for Curtain Wall Frames
- Gitae Park, Seunggab Hong, Kyongyun Yeau, Boyoung Jeong
- J Weld Join. 2022;40(6):485-495.
-
Research Papers
Metallurgical Factors Affecting the Tensile Properties of Weld Heat-Affected Zone in Medium Mn Transformation-Induced Plasticity Steel
- Gitae Park
- J Weld Join. 2022;40(4):329-336.
-
Review Papers
Review on the Resistance Spot Weldability of Medium-Mn TRIP steel
- Gitae Park, Sangho Uhm, Changhee Lee
- J Weld Join. 2021;39(3):239-245.
-
Research Papers
Microstructure and Mechanical Properties of Reheated Zones
in the Multi-pass Weld Metal of High-Strength Steel
- Yongjoon Kang, Gitae Park, Seonghoon Jeong, Changhee Lee
- J Weld Join. 2017;35(6):21-26.