Research Papers
Comparative Analysis of SPR and SPR-Bonded Joints of Hot Press Forming Steel and AA5052 under Corrosive Conditions
- Han-ju Lee, Savyasachi Nellikode, Tae-Young Kang, Yeong-Do Park
- J Weld Join. 2023;41(6):486-499.
-
Research Papers
Effect of Top Sheet Materials on Joint Performance of Self-Piercing Riveting
- Md Abdul Karim, Siva Prasad Murugan, KiMan Bae, Jongjin Baek, Changwook Ji, Wooram Noh, Han-Ju Lee, Will Jang, Duck Bong Kim, Yeong-Do Park
- J Weld Join. 2022;40(6):512-524.
-
Research Papers
Study on Effect of Process Variable on Fastening Quality Using Process Monitoring Data of Flow Drill Screwed 590DP Steel/AA5052 combination
- Tae-Young Kang, Han-ju Lee, Karim Md Abdul, Dae-Geun Nam, Byeong-ryong Lee, Jung-Muk Choi, Yeong-Do Park
- J Weld Join. 2022;40(3):256-264.