Research Papers
A Study on the Establishment of Alternative Verification Standard of Ballistic Ttest for Armored Steel Arc Welding Procedure
- Yong Kim, Min Chul Oh, Ji Young Jang, Do Hui Kim
- J Weld Join. 2024;42(1):125-133.
-
Research Papers
Study on Laser Welding of Dissimilar Materials between Aluminum and Copper (Ⅰ) - Research Trend in Laser Welding Technology and Materials Testing Methods -
- Yong Kim, Su Jin Jeong, Seong Min Yun, Je In Lee
- J Weld Join. 2022;40(5):416-437.
-
Research Papers
Joining Technologies and Solutions for Aluminum-based Battery Case Manufacturing
- Yong Kim, Yeong-Do Park
- J Weld Join. 2022;40(1):54-73.
-
Research Papers
Microstructure and Mechanical Properties of Friction-Welded Alloy 718 and SNCRW Stainless Steel After Post-Weld Heat-Treatment
- Jeoung Han Kim, Nam-Yong Kim, Yu Sik Kong, Nho Kwang Park
- J Weld Join. 2019;37(4):313-317.
-
Review Papers
Recent Joining Techniques of CFRP to Metal Using Welding Process
- Yong Kim, Hee-seon Bang
- J Weld Join. 2018;36(5):27-38.
-
Research Papers
Recent Trends about Modulation Technology of the Laser Beam Welding
- Yong Kim, Cheolhee Kim
- J Weld Join. 2018;36(4):47-57.
-
Research Papers
A Study on the Dissimilar Metal Joining of Aluminum to Steel Using the Arc Heat Source (Ⅳ) - Fatigue Behaviors Using Ultrasonic Elastic Resonance -
- Yong Kim, Jae-Seong Kim, In-Sik Cho, Bo-Young Lee
- J Weld Join. 2018;36(4):36-46.
-
Research Papers
A Study on the Dissimilar Metal Joining of Aluminum to Steel Using the Arc Heat Source (Ⅲ) - Static Strength and Fracture Behaviors -
- Yong Kim, Cheolhee Kim, Bo-Young Lee
- J Weld Join. 2018;36(4):23-35.
-
Research Papers
A Study on the Dissimilar Metal Joining of Aluminum to Steel Using the Arc Heat Source (Ⅱ) - Mechanism of Dissimilar Metal Joining -
- Yong Kim, Ki-Young Park, Bo-Young Lee
- J Weld Join. 2018;36(4):13-22.
-
Research Papers
A Study on the Dissimilar Metal Joining of Aluminum to Steel Using the Arc Heat Source (Ⅰ) - Research Trends and Comparison of the Processes -
- Yong Kim, Bo-Young Lee
- J Weld Join. 2018;36(4):1-12.
-
Research Papers
Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel
- Yong Kim
- J Weld Join. 2017;35(5):16-22.
-
Review Papers
Mechanical fastening and joining technologies to using multi mixed materials of car body
- Yong Kim, Ki-Young Park, Sung-Bok Kwak
- J Weld Join. 2015;33(3):12-18.
-
Research Papers
Optimization of arc brazing process parameters for exhaust system parts using box-behnken design of experiment
- Yong Kim, Pyeong-Won Park, Ki-Young Park, Jin-Chul Ryu
- J Weld Join. 2015;33(2):23-31.
-
Research Papers
Degradation Behavior of Eutectic and Pb-free Solder Plated Ribbon in Crystalline Silicon Photovoltaic Module
- Ju-Hee Kim, A Yong Kim, Nochang Park, Jeong Won Ha, Sang Guon Lee, Won Sik Hong
- J Weld Join. 2014;32(6):611-617.
-
Technical reports
A Study on Laser Weldability of Al-Si Coated 22MnB5 Steel for TWB Hot Stamping
- Yong Kim, Ki-Young Park, Bo-Young Lee
- Journal of KWJS. 2013;31(2):30-36.
-
Micro TIG Welding Characteristics of Stainless Steel Bellows
- Yong Kim, Ki-Young Park
- Journal of KWJS. 2012;30(2):11-15.
-
Methods for Fatigue Strength Improvement of the Weld Structure (Ⅱ) - Post Weld Improvement Methods
- Yong Kim, Bo-Young Lee
- Journal of KWJS. 2012;30(2):1-4.
-
Methods for Fatigue Strength Improvement of the Weld Structure (Ⅰ) - Design of Welded Joints
- Yong Kim, Bo-Young Lee
- Journal of KWJS. 2012;30(1):5-7.
-
Development of Welding Technologies for Lightweight Vehicle
- Yong Kim, Ki-Young Park, Kyoung-Don Lee
- Journal of KWJS. 2011;29(6):1-3.
-
Evaluation of Formability Depend on Aluminum Filler Wire to Make Lightweight Vehicle for MIG Welding Process
- Yong Kim, Ki-Young Park, Kyoung-Don Lee
- Journal of KWJS. 2011;29(4):30-34.
-
Laser Welding Characteristics of 1.5㎬ Grade Hot Stamping Steel for Automobiles
- Yong Kim, Ki-Young Park, Kyoung-Don Lee
- Journal of KWJS. 2010;28(6):4-9.
-
Steel to Aluminum Joining by Arc Process
- Yong Kim, Ki-Young Park, Kyoung-Don Lee
- Journal of KWJS. 2010;28(5):1-3.
-
The Development and Application of Intelligent Welding Carriage with High Deposition Rate by 3-D Weaving
- Young-Zoo Kim, Bang-Hyun Cho, Amit, Sang-Bum Lee, Weon-Gu Lee, Jin-Yong Kim, Man-Joo Huh
- Journal of KWJS. 2010;28(2):32-38.
-
Optimum Design of the Friction Stir Welding Process on A6005 Extruded Alloy for Railway Vehicles to Improve Mechanical Properties
- Si-Tea Won, Weon-Kyong Kim
- Journal of KWJS. 2009;27(5):81-87.
-
Study on the Effects of Flows on the Acceleration of the Grooving Corrosion in the ERW Pipe
- Jae-Seong Kim, Yong Kim, Bo-Young Lee
- Journal of KWJS. 2008;26(4):85-91.
-
Development the Technique for Fabrication of the Thermal Fatigue Crack to Enhance the Reliability of Structural Component in NPPs
- Yong Kim, JaeSung Kim, BoYoung Lee
- Journal of KWJS. 2008;26(2):43-49.
-
Effects of Nd:YAG Laser Welding Parameters on Fatigue life of Lap Joint Structure in Stainless Steel
- Yong Kim, Hyun-Seok Yang, Ki-Young Park, Kyoung-Don Lee
- Journal of KWJS. 2008;26(1):69-75.
-
A Study on Grooving Corrosion at the Weld of a Low Carbon Steel Pipe Made by Electrical Resistance Welding
- Yong Kim, Bo-Young Lee
- Journal of KWJS. 2004;22(5):58-64.