J Weld Join. 2014;32(1):15-21. Published online February 27, 2014.
DOI: https://doi.org/10.5781/JWJ.2014.32.1.15
- Evaluation on Mechanical Properties with Welding Processes for Off Shore Wind Tower Application
-
Changwook Ji*, Chul Young Choi*, Dae-Geun Nam**, Hyoung Chan Kim**, Jae Ho Jang**, Ki Hyuk Kim***, Yeong-Do Park****
-
- Corresponding author: Yeong-Do Park ,Email: ypark@deu.ac.kr
- Abstract
- FCAW(Flux Cored Arc Welding), SAW(Submerged Arc Welding), EGW(Electro Gas Welding), and three-pole SAW are applicable in manufacturing the offshore wind tower. In this paper, mechanical properties of these welded-joints for TMCP steels were evaluated in all above welding processes. The tensile strength of welded-joints for all the welding methods satisfied the standard guideline (KS D 3515). No cracking on weldment was found after the bending test. Changes of weldedments hardness with welding processes were observed. In a weld HAZ (heat-affected zone), a softened HAZ-zone was formed with high heat input welding processes (SAW and EGW). However, the welded-joint fractures were found in the base metal for all cases and small decrease in welded-joint strength was caused by a softened zone. The multi-pole SAW welds exhibited similar mechanical properties comparing to the one with one-pole SAW process.
Keywords :FCAW, SAW, EGW, Wind tower, TMCP