Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88
Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89
-
9
-
J Weld Join. 2014;32(1):40-46. Published online February 27, 2014.
DOI: https://doi.org/10.5781/JWJ.2014.32.1.40
- Bonding Mechanism and Strength of Metals to Ceramics
-
Se-Ho Kee*, Jae-Pil Jung*, Won-Joong Kim*
-
- Corresponding author: Won-Joong Kim ,Email: wjkim@uos.ac.kr
- Abstract
- Bonding technology and bonding mechanism of metal to ceramic including brazing, diffusion bonding, friction welding and etc were reviewed in this study. Various factors should be considered from a bonding design step to acquire a good bonding joint because of a large difference between metal and ceramic in crystal lattice, coefficient of thermal expansion and various properties. In addition, metal and ceramic bonding technologies are constantly being developed according to precise components, multi-function and application to harsh environment. However, improvement of bonding properties and bonding reliability also should be accompanied. Bonding of ceramics, such as ZrO2, Ti3AlC2 and SiC, to metals like Ti-alloy, TiAl and steel were described in this paper.
Keywords :Active metal brazing, Ceramics, Bonding mechanism, Wettability, Residual stress