J Weld Join. 2014;32(3):257-266. Published online June 30, 2014.
DOI: https://doi.org/10.5781/JWJ.2014.32.3.43
- Recent Study of Thermal Spray for Green Automotive Industry
-
Ho-Cheon Yoo*,†
-
- Corresponding author: Ho-Cheon Yoo ,Email: yooho278@reseat.re.kr
- Abstract
- Recent developing tendency of thermal spray for green automotive industry are studied by searching of
NDSL, KIPRIS, ScienceDirect and so on. Spraying techniques such as plasma spray, microwave treatment,
dry-ice blasting, HVOF thermal spray, cold spraying, aerosol deposition are introduced, further more spraying
materials such as nano particles, intermetallic compound, TiAlN, TiC, Si-Al alloys are investigated.
Keywords :Thermal spray, Automotive, Plasma spray, Intermetallic compound, Cold spraying, HVOF