Optimization of Painting Process to Improve Durability of Mega Yacht and Cavitation Erosion Characteristics
Il-Cho Park, Min-Su Han, Seong-Jong Kim
J Weld Join. 2019;37(3):254-261.   Published online June 10, 2019
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Effect of BOE Wet Etching on Interfacial Characteristics of Cu-Cu Pattern Direct Bonds for 3D-IC Integrations
Jong-Myeong Park, Su-Hyeong Kim, SarahEunkyung Kim, Young-Bae Park
J Weld Join. 2012;30(3):26-31.   Published online July 18, 2012
PDFPDF    
Adhesion Measurement Methods for Thin Films in Microelectronics
Taek-Soo Kim
J Weld Join. 2012;30(3):15-20.   Published online July 18, 2012
PDFPDF    
A Study on the Adhesive Characteristics of Nano Scale Particles Considering Asperity Interaction
Chang-Hun Lee, Kyong-Hun Lee, Jun-Ho Yoon, Young-Eui Shin
J Weld Join. 2008;26(1):56-62.   Published online March 21, 2008
PDFPDF    
Characteristics of Plasma Sprayed TiO₂-NiCr Conductive Heating Roll Coatings
Tae-Gu Kang, Min-Seok Jin, Young-Bong Ko et al.
J Weld Join. 2007;25(4):28-34.   Published online September 21, 2007
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI