2031583
Heat Treatment Effect on Super Duplex Stainless Steel UNS S32750 FCA Multipass Welds
Bok-Su Jang, In-June Moon, Myung-Jin Lim et al.
J Weld Join. 2014;32(2):174-179.   Published online May 14, 2014
PDFPDF    
Laser Beam Welding Technology of Seal Tube for Radiation-Resistant LVDT Manufacturing
Soo-Sung Kim, Chul-Yong Lee, Kee-Nam Choo, Jin-Hyun Koh
J Weld Join. 2011;29(5):4-10.   Published online November 22, 2011
PDFPDF    
Application of Welding Technology for a Zirconium Alloy of Nuclear Fuel Cladding
Soo-Sung Kim, Jin-Hyun Koh, Jung-Won Lee, Geun-Il Park
J Weld Join. 2011;29(1):5-8.   Published online March 4, 2011
PDFPDF    
Development of Remote Resistance Welding Equipment for Nuclear Fuel Multi-pin Fabrication
Jin-Hyun Koh, Soo-Sung Kim
J Weld Join. 2006;24(6):1-4.   Published online February 12, 2007
PDFPDF    
Improvement of LBW quality of Zircaloy-4 Spacer Grids for PWR Fuel Assembly
Soo-Sung Kim, Kee-Nam Song, Hyoung-Jun Han
J Weld Join. 2006;24(5):22-28.   Published online January 4, 2007
PDFPDF    
Laser Welding of Seal Tube for Instrumented Irradiation Fuel Test
Soo-Sung Kim, Chul-Yong Lee, Woong-Ki Kim, Geun-Il Park, Jinh-Yun Koh, Jun-Seok Seo
J Weld Join. 2005;23(6):43-48.   Published online January 26, 2006
PDFPDF    
Technology of the End Cap Laser Welding for Irradiation Fuel Rods
Soo-Sung Kim, Jung-Won Lee, Jin-Hyun Koh, Young-Ho Lee
J Weld Join. 2003;21(6):20-25.   Published online October 27, 2003
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI