Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 An Assessment of the Accuracy for Digital Radiography Image

Journal of KWJS 2009;27(2):51-56.
Published online May 18, 2009.
디지털 방사선투과영상의 정밀성 평가에 관한 연구
, ,
 
An Assessment of the Accuracy for Digital Radiography Image
Sang-Ki Park, Yean-Shik Ahn, Doo-Song Gil
Abstract
  Film based radiography imaging technique has been applied to the non-destructive test in medical, aircraft, and power industries contributing to the development of the industries.
  However, the complex process for imaging and analysis has increasingly demanded the reformation of the radiography test. A digital radiography imaging technologies has been com out from the demand. This study was mainly focused on the assessment on the accuracy for the each image from digital radiography test and film radiography test was proven to crate a better image in sensitivity than film radiography test. In the IQI (Image quality indicator) transmission test, one or two more line can be seen in digital image than in film image.
  When applying to the boiler tube weld, film image is detectable to the 1.0㎜ depth flaw; and digital image to the 0.5㎜ depth flaw. As a result of this study, digital radiography technology is determined to enhance the image quality, compared to film radiography technologies
Key Words: Non-destructive test, Digital radiography, Welding inspection
TOOLS
METRICS Graph View
  • 1,478 View
  • 0 Download
Related articles


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI