Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Effect of Post Weld Heat Treatment for Crystal Orientation Distribution on Friction Stir Welds of Al-Mg-Si Series Aluminum Alloy Sheets

Journal of KWJS 2009;27(6):62-67.
Published online January 13, 2010.
Al-Mg-Si계 알루미늄 합금 판재 마찰교반접합부의 결정 방위 분포에 대한 용접후열처리의 영향
 
Effect of Post Weld Heat Treatment for Crystal Orientation Distribution on Friction Stir Welds of Al-Mg-Si Series Aluminum Alloy Sheets
Kwang-jin Lee
Abstract
  Friction stir welding (FSW) was carried out for Al-Mg-Si series aluminum alloys which are being used for automotive body structure. Consequently, Post weld heat treatment (PWHT) was applied to the friction stir welds to evaluate the effect of the paint baking process which is one of the automotive fabrication process on friction stir welded zone (FSWZ) in 443K for 1.2Ks. Grain structure and its crystal orientation distribution was measured about both the as welded specimens and the post weld heat treated specimens. An optical microscope (OM) and an field emission scanning electron microscope (FE-SEM) was used for observing the grain structure and measuring its crystal orientation distribution, respectively. Changes on the grain structure and its crystal orientation distribution were not detected. From the present results, it was confirmed that the paint baking process after FSW do not affect on the grain structure and its crystal orientation distribution of FSWZ. The comprehensive investigations will be performed for various automotive aluminum alloys manufactured by different processes, in the future.
Key Words: Al-Mg-Si series aluminum alloy, FSW, PWHT, Crystal orientation distribution


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI