Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Comparison Study for the Shear Strength of the Bondings between Stainless Steel Crown/Direct Type Composite Resin and Stainless Steel Crown/Indirect Type Composite Resin

Journal of KWJS 2011;29(4):93-99.
Published online September 12, 2011.
치과 치료학에서 적용되는 접합기술 연구 ; 스테인리스강 크라운에 접합된 직접용 콤포짓트 레진과 간접용 콤포짓트 레진의 전단결합강도 비교
,
 
Comparison Study for the Shear Strength of the Bondings between Stainless Steel Crown/Direct Type Composite Resin and Stainless Steel Crown/Indirect Type Composite Resin
Gwangsoo Kim, Kwangwoo Baek
Abstract
  This study was performed to compare the shear strength of the bondings between stainless steel crown/direct type composite resin and stainless steel crown/indirect type composite resin. Four groups of bonding conditions were prepared. Two groups of bonding conditions were made by the indirect type composite resin system and the other two groups were made by the direct type composite resin system. The shear strength tests were carried out using universal testing machine, Model 4465 of Instron Co.. It was indicated that the bond strength values of the indirect type composite resins were higher than those of the direct type composite resins. TE-SE group was superior to the TE-ONE in indirect type resin system. These results were thought to be the high degree of the polymerization accompanied with temperature and pressure of the resin of indirect type resin. It was also found that indirect composite resin contains less amount of porosity in resin.
Key Words: Shear strength, Stainless steel crown, Composite resin
TOOLS
METRICS Graph View
  • 1,698 View
  • 0 Download
Related articles


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI