Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Using Neural Network Algorithm for Bead Visualization

J Weld Join > Volume 31(5); 2013 > Article
Journal of KWJS 2013;31(5):35-40.
DOI: https://doi.org/10.5781/KWJS.2013.31.5.35    Published online November 5, 2013.
Using Neural Network Algorithm for Bead Visualization
Chang-Dae Koo1, Hyeong-Seok Yang1, Jung-Yeong Kim2, Sang-Ho Shin3
Correspondence:  Sang-Ho Shin,
Email: shinsky@tsb.co.kr
Abstract
In this paper, we propose the Tangible Virtual Reality Representation Method to using haptic device and feature to morphology of created bead from Flux Cored Arc Welding. The virtual reality was started to rising for reduce to consumable materials and welding training risk. And, we will expected maximize virtual reality from virtual welding training. In this paper proposed method is get the database to changing the input factor such as work angle, travelling angle, speed, CTWD. And, it is visualization to bead from extract to optimal morphological feature information to using the Neural Network algorithm. The database was building without error to extract data from automatic robot welder. Also, the Neural Network algorithm was set a dataset of the highest accuracy from verification process in many times. The bead was created in virtual reality from extract to morphological feature information. We were implementation to final shape of bead and overlapped in process by time to using bead generation algorithm and calibration algorithm for generate to same bead shape to real database in process of generating bead.
The best advantage of virtual welding training, it can be get the many data to training evaluation.
In this paper, we were representation bead to similar shape from generated bead to Flux Cored Arc Welding. Therefore, we were reduce the gap to virtual welding training and real welding training. In addition, we were confirmed be able to maximize the performance of education from more effective evaluation system
Key Words: Neural network algorithm, Virtual welding, Bead visualization
TOOLS
METRICS Graph View
  • 0 Crossref
  •    
  • 2,137 View
  • 5 Download
Related articles


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI