Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Development of New Low Frequency ECT Sensor to Detect Inner Defects(I) - Characteristic of Loss of Induced Electromotive Force -

J Weld Join > Volume 33(4); 2015 > Article
Journal of Welding and Joining 2015;33(4):57-62.
DOI: https://doi.org/10.5781/JWJ.2015.33.4.57    Published online August 31, 2015.
Development of New Low Frequency ECT Sensor to Detect Inner Defects(I) - Characteristic of Loss of Induced Electromotive Force -
Jeong-Ung Park*, Mun-Seok Jang**, Guk-Ju Gim***, Beom-Ki Kim***
Correspondence:  Jeong-Ung Park,
Email: jupark@chosun.ac.kr
Abstract
Non-destructive techniques are used widely in the metal industry in order to control the quality of materials. Eddy current testing(ECT) is one of the most extensively used non-destructive techniques for inspecting electrically conductive materials at very high speeds that does not require any contact between the test piece and the sensor. The New ECT sensor which can detect inner defects was developed regardless the condition of surface. This sensor is verified to do experiment which measure the loss of induced electromotive force. The loss of induced electromotive force was measured in 5.4% and this low frequency ECT device can detect internal defects at depth 20 mm.
Key Words: Non-destructive techniques, Eddy current testing, Loss of induced electromotive force, Low frequency ECT


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI