Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 오스테나이트계 스테인레스강 용접부의 DELTA-FERRITE 생성인자

Journal of KWJS 1987;5(1):16-22.
Published online March 25, 1987.
오스테나이트계 스테인레스강 용접부의 DELTA-FERRITE 생성인자
,
 
오스테나이트계 스테인레스강 용접부의 DELTA-FERRITE 생성인자
문영훈, 허성도