Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 The Effect of PWHT on Fatigue Fracture in HAZ of Cr-Mo Steel : ( for heating rate )

Journal of KWJS 1987;5(1):73-80.
Published online March 25, 1987.
Cr-Mo강 용접후 열처리재의 피로파괴에 관한 연구 ( 가열속도를 중심으로 )
, ,
 
The Effect of PWHT on Fatigue Fracture in HAZ of Cr-Mo Steel : ( for heating rate )
임재규, 정세희, 최동암