Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Study on the Estimation of Environmental Strength in Welded of Steels in Seawater ( II ) - Corrosion Fatigue Crack Growth Behaviours for Low Cycle -

Journal of KWJS 1989;7(1):51-58.
Published online March 27, 1989.
해수환경에서 강 용접부의 환경강도평가에 관한 연구 ( II ) - Low Cycle 부식피로균열진전거동 -
, , ,
 
Study on the Estimation of Environmental Strength in Welded of Steels in Seawater ( II ) - Corrosion Fatigue Crack Growth Behaviours for Low Cycle -
나의균, 임재규, 조규종, 정세희