Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Brazing of Aluminium Nitride ( AIN ) to Copper with Ag-based Active Filler Metals

Journal of KWJS 1995;13(3):134-146.
Published online September 25, 1995.
은 ( Ag ) 계 활성금속을 사용한 질화 알미늄 ( AIN ) 과 Cu의 브레이징
, ,
 
Brazing of Aluminium Nitride ( AIN ) to Copper with Ag-based Active Filler Metals
허대, 김대훈, 천병선