Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Improvement of Powder Feeding Characteristics of Fine ( 5 μm ) Al2O3 Powder by Modification of the Powder Feeding Systems and Characterization of the Coating Layer depending on Plasma Spraying Conditions

Journal of KWJS 1997;15(1):116-124.
Published online February 25, 1997.
분말송급장치의 개조에 의한 미세 ( 5 μm ) Al2O3 분말의 송급특성개선 및 플라즈마 용사조건에 따른 코팅층의 특성분석
, , , ,
 
Improvement of Powder Feeding Characteristics of Fine ( 5 μm ) Al2O3 Powder by Modification of the Powder Feeding Systems and Characterization of the Coating Layer depending on Plasma Spraying Conditions
설동욱, 김병희, 정민석, 임영우, 서동수
TOOLS
METRICS Graph View
  • 1,232 View
  • 0 Download
Related articles


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI