Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 A Study on High Temperature Crack Growth Behavior in 2.25Cr-1Mo Steel Weldments at 550℃

Journal of KWJS 2001;19(3):27-33.
Published online June 25, 2001.
550℃에서의 2.25Cr-1Mo강 용접부의 고온 균열성장 거동에 관한 연구
, ,
 
A Study on High Temperature Crack Growth Behavior in 2.25Cr-1Mo Steel Weldments at 550℃
김호경, 정강, 정진성