Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 A Study on Cyclic Bending Load of Bus Folding Door Pillar including Adhesive Bonding and Spot Welding

Journal of KWJS 2006;24(3):55-59.
Published online August 22, 2006.
접착제 접합과 점용접된 버스 폴딩도어 필러의 굽힘피로강도 평가에 관한 연구
 
A Study on Cyclic Bending Load of Bus Folding Door Pillar including Adhesive Bonding and Spot Welding
Ho-Chel Yoon
Abstract
  This paper is concerned with a study on cyclic bending load of bus folding door pillar including adhesive bonding and spot welding. Three specimen types were used such as spot welding, I-type adhesive bonding and M-type adhesive bonding in this study. The tensile-shear tests were carried out to evaluate the tensile-shear strength of these three specimen types. Also four-point bending tests were carried out to evaluate the static and dynamic bending load. From the results, using adhesive bonding has a better effect on the static and dynamic bending load than using spot welding. Therefore, manufacturing better structural products can be expected by applying hybrid welding using adhesive and spot welding to those.
Key Words: Bus folding door pillar, Cyclic Bending load, Adhesive bonding, Spot welding
TOOLS
METRICS Graph View
  • 1,500 View
  • 0 Download
Related articles

A Study on Effects of Welding Clearance on Spot Weldability 2002 February;20(1)



ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI