스테인리스강 Spot 용접부의 산화방지에 관한 연구
,
 
A Study on Anti-Oxidation of Stainless Steel Spot Weld
DongWoon Huh, Sehun Rhee
Abstract
  Stainless steels are alloy steels with a nominal chromium content of at least 11 percent, with other alloy additions. The stainlessness and corrosion resistance of these alloy steels are attributed to the presence of a passive oxide film on the surface. When exposed to conditions like Resistance Spot Welding (RSW) process that remove the passive oxide film, stainless steels are subject to corrosive attack. And exposure to elevated temperatures causes oxidation (discoloration) of areas around indentation in Spot welding. In this paper, deal with the effect of shielding gas (Ar) preventing the corrosion, oxidation of stainless steel. And find the optimal shielding gas flow rate. In addition, suggest effective purging method for direct/indirect spot welding process.
Key Words: Resistance Spot Welding(RSW), Anti-oxidation, Shielding gas, Stainless steel passive oxide film


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI