Journal of Welding and Joining 2015 December;33(6) :55-59.
Published online December 31, 2015.
doi:https://doi.org/10.5781/JWJ.2015.33.6.55
Design of Helical SPR for Joining Advanced High Strength Steel and Aluminum Alloy Sheets
Dongbum Kim*, Kwan-Woo Kim*, Hae-Yong Cho*
*Dept. of Mechanical Engineering, Chungbuk National University, Cheongju 362-763, Korea
Correspondence: Hae-Yong Cho  Email: hycho@chungbuk.ac.kr
  Published online December 31, 2015
ABSTRACT
Self-piercing riveting (SPR) is a sheet-joining method that can be used for materials that are difficult or unsuitable for weld, such as aluminum alloys and other steel sheet metals. The increased application of lightweight materials has initiated many investigations into new SPR conditions for riveting dissimilar materials. However, buckling of the semi-tubular rivet occurs during the riveting of AHSS. In this study, a helical SPR was designed for the riveting of AHSS and Al-alloy. In addition, the reinforced helical SPR which has straight parts was designed. The riveting of AHSS and Al-alloy was simulated. Simulated results were verified by comparison with experimental ones.
Keywords: Self-piercing riveting(SPR) | Helical SPR | Advanced high strength steels(AHSS) | SILAFONT | Finite element analysis(FEA) | CP1470
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
2
Crossref
1,683
View
23
Download
Related articles
A Review of Joining Processes for High Strength 7xxx Series Aluminum Alloys  2017 December;35(6)
Development of Durability Enhancement Technology for Arc Weldings in Advanced High Strength Steel (AHSS) Chassis Parts   2015 August;33(4)
Design of self-piercing rivet to joint in advanced high strength steel and aluminium alloy sheets  2015 June;33(3)
Development of Thermite Powder for Rail Joining with Recycled Iron Oxide and Aluminium Powder  2012 October;30(5)
Evaluation of Hydrogen Delayed Fracture for High Strength Steels and Weldments  2011 December;29(6)
A Review of Joining Processes for High Strength 7xxx Series Aluminum Alloys  2017 December;35(6)
Development of Durability Enhancement Technology for Arc Weldings in Advanced High Strength Steel (AHSS) Chassis Parts   2015 August;33(4)
Design of self-piercing rivet to joint in advanced high strength steel and aluminium alloy sheets  2015 June;33(3)
Development of Thermite Powder for Rail Joining with Recycled Iron Oxide and Aluminium Powder  2012 October;30(5)
Evaluation of Hydrogen Delayed Fracture for High Strength Steels and Weldments  2011 December;29(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI