Previous issues
Volume 35 Issue 5
-
Research Papers
Corrosion Assessment for Boron Steel Weldments Prepared by Overlap Welding and Successive Hot Press Forming Processes
- Minjung Kang, Cheolhee Kim
- J Weld Join. 2017;35(5):1-6.
-
Research Papers
Hot Cracking of Ni-Cr-Fe Alloys: Test Methods and Metallurgical Effect
- Sangwoo Nam, Cheolhee Kim, Young-Min Kim
- J Weld Join. 2017;35(5):7-15.
-
Research Papers
Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel
- Yong Kim
- J Weld Join. 2017;35(5):16-22.
-
Research Papers
A Study of Characteristics of Vertical-up SMA Welding by Short Circuit Control
- Kyung-Hun Lee, Hoi-Soo Ryoo, Soong-Keun Hyun
- J Weld Join. 2017;35(5):23-28.
-
Research Papers
MIG Welding Optimization of Muffler Manufacture by Microstructural Change and
Thermal Deformation Analysis
- Seung Ho Lee, Eok Soo Kim, Jin-Young Park, Jun Choi
- J Weld Join. 2017;35(5):29-37.
-
Research Papers
Thermal Aging Characteristics of Sn-xSb Solder for Automotive Power Module
- Junhyuk Son, Minkyung Kim, Dong-Yurl Yu, Young-Ho Ko, Jeong-Won Yoon, Chang-Woo Lee, Young-Bae Park, Junghwan Bang
- J Weld Join. 2017;35(5):38-47.
-
Research Papers
The Changes of Chemical Composition and Microstructure in Electroslag Cladding
Overlays by using AISI 430 Stainless Steel Strip
- Jae-Young Jung, Tae-Kwon Ha
- J Weld Join. 2017;35(5):48-56.
-
Research Papers
Development of Printed Circuit Heat Exchanger for Hydrogen Station using Diffusion Bonding
- Jeong Kil Kim, Deog Nam Shim, Chil Yeong Seon, Ki Hoon Yang, Hae Ji Park, Dong Jin Kim
- J Weld Join. 2017;35(5):57-64.
-
Research Papers
Effects of Fluoride in the Flux on Hydrogen Content in Weld Metal and Operating Behavior in FCAW-S
- Woong Kil, Myeong-jun Shin, Kook-soo Bang
- J Weld Join. 2017;35(5):65-70.
-
Research Papers
The Study on Characteristics of Dissimilar Weld Metals between AA6061-T6 and Silafont-36 by Laser Welding
- Jun-Hyeok Hyun, Tae-Woo Shin, Bok-Su Jang, Sang-Ho Kim, Gun-Ho Go, Tae-Young Kim, Jin-Hyun Koh
- J Weld Join. 2017;35(5):71-76.
-
Research Papers
Effects of Welding Parameters on the Overlay Welding Behaviors in Electroslag Cladding
by using AISI 430 Stainless Steel Strip - Experimental Study
- Jae-Young Jung, Tae-Kwon Ha
- J Weld Join. 2017;35(5):77-86.