Study on the Initial Design of an LNG Fuel Tank using 9 wt.% Nickel Steel for Ships and Performance Evaluation of the Welded Joint
Bo Eun Kim, Jeong-Yeol Park, Jeong Soo Lee, Myung-Hyun Kim
J Weld Join. 2019;37(6):555-563.