Research Papers
Non-Destructive Testing of Laser Welded Hydrogen Storage Tank Liner Using Optical Coherence Tomography
Ryoonhan Kim, Dongsig Shin, Sujin Lee, Danbi Song, Sang-Eon Park, Wooyoung Chung, Sangbae Han
J Weld Join. 2024;42(1):99-105.