Research Papers
Prediction of Weld Tensile-Shear Strength using ANN Based on the Weld Shape in Aluminum Alloy GMAW
- Dong-Yoon Kim, June Hyung Hwang, Gwang-Gook Kim, Young-Min Kim, Jiyoung Yu, Junhong Park
- J Weld Join. 2023;41(1):17-27.
-
Research Papers
Convolutional Neural Network Model for the Prediction of Back-Bead Occurrence in GMA Root Pass Welding of V-groove Butt Joint
- Hyung Won Lee, Jiyoung Yu, Gwang-Gook Kim, Young-Min Kim, Insung Hwang, Seung Hwan Lee, Dong-Yoon Kim
- J Weld Join. 2021;39(5):463-470.