-
Research Papers
Experimental Investigations into Improvement of Cleaning Performance for Anticorrosive Paints for Shipbuilding using Handheld-Type Laser Cleaning Equipment
- Ji-Eon Kim, Moo-Keun Song, Jong-Myoung Lee, Jeong-Hun Hyun, Gi-Hun Lee, Jong-Do Kim
- J Weld Join. 2021;39(5):536-541.
-
Research Papers
A Fundamental Study on the High-Power Fiber Laser Cleaning for Removing the Multi-Layer Coating
- Jong-Do Kim, Ji-Eon Kim, Moo-Keun Song, Jong-Myoung Lee
- J Weld Join. 2020;38(6):563-568.
-
Research Papers
A Study on the Effect of Overlap Rate on Laser Beam Cleaning Characteristics while Cleaning Paint Using a Low Power Pulsed Laser(Ⅰ) - Analysis of Laser Cleaned Surface Characteristics Based on Number of Scans -
- Ji-Eon Kim, Moo-Keun Song, Jong-Myoung Lee, Jeong-Hun Hyun, Jong-Do Kim
- J Weld Join. 2019;37(5):435-440.
-
Research Papers
A Study on the Effect of Overlap Rate on Laser Beam Cleaning Characteristics while Cleaning Paint Using a Low Power Pulsed Laser(Ⅱ) - Analysis of Laser Cleaned Surface Characteristics for Various Pulse Overlap Rates -
- Ji-Eon Kim, Moo-Keun Song, Jong-Myoung Lee, Jeong-Hun Hyun, Jong-Do Kim
- J Weld Join. 2019;37(5):441-447.