Research Papers
The Effect of PWHT on the Characteristics of Duplex Stainless Steel
(ASTM A240 UNS S31803) Weld Metals made with FCAW
- Jun-Hyeok Hyun, Tae-Woo Shin, Bok-Su Jang, Sang-Ho Kim, Jin-Hyun Koh
- J Weld Join. 2017;35(6):89-95.
-
Research Papers
The Study on Characteristics of Dissimilar Weld Metals between AA6061-T6 and Silafont-36 by Laser Welding
- Jun-Hyeok Hyun, Tae-Woo Shin, Bok-Su Jang, Sang-Ho Kim, Gun-Ho Go, Tae-Young Kim, Jin-Hyun Koh
- J Weld Join. 2017;35(5):71-76.