Research Papers
Effect of Assistant Gas Pressure on Cutting Performance when 80mmt Stainless Steel Laser Cutting in Pressurized Underwater Environment
- Jaeook Jeon, Moo-Keun Song, Kwan Kim, Sujin Lee, Dae-won Cho, Dongsig Shin, Jongdo Kim
- J Weld Join. 2023;41(6):540-547.
-
Research Papers
Experimental Investigations into Improvement of Cleaning Performance for Anticorrosive Paints for Shipbuilding using Handheld-Type Laser Cleaning Equipment
- Ji-Eon Kim, Moo-Keun Song, Jong-Myoung Lee, Jeong-Hun Hyun, Gi-Hun Lee, Jong-Do Kim
- J Weld Join. 2021;39(5):536-541.
-
Research Papers
A Fundamental Study on the High-Power Fiber Laser Cleaning for Removing the Multi-Layer Coating
- Jong-Do Kim, Ji-Eon Kim, Moo-Keun Song, Jong-Myoung Lee
- J Weld Join. 2020;38(6):563-568.
-
Research Papers
A Study on the Effect of Overlap Rate on Laser Beam Cleaning Characteristics while Cleaning Paint Using a Low Power Pulsed Laser(Ⅰ) - Analysis of Laser Cleaned Surface Characteristics Based on Number of Scans -
- Ji-Eon Kim, Moo-Keun Song, Jong-Myoung Lee, Jeong-Hun Hyun, Jong-Do Kim
- J Weld Join. 2019;37(5):435-440.
-
Research Papers
A Study on the Effect of Overlap Rate on Laser Beam Cleaning Characteristics while Cleaning Paint Using a Low Power Pulsed Laser(Ⅱ) - Analysis of Laser Cleaned Surface Characteristics for Various Pulse Overlap Rates -
- Ji-Eon Kim, Moo-Keun Song, Jong-Myoung Lee, Jeong-Hun Hyun, Jong-Do Kim
- J Weld Join. 2019;37(5):441-447.
-
Research Papers
A Study on the Characteristics of Laser Cladding Using the LC-190 Cemented Carbide Powder(I)
- Characteristic Analysis of One-pass Clad Layer with Parameters -
- Jong-Do Kim, Su-Han Park, Moo-Keun Song
- J Weld Join. 2018;36(6):34-39.
-
Research Papers
A Study on the Characteristics of Laser Cladding Using the LC-190 Cemented Carbide Powder(II)
- Characteristic Analysis of Multi-pass Clad Layer -
- Jong-Do Kim, Su-Han Park, Moo-Keun Song
- J Weld Join. 2018;36(6):40-45.
-
Research Papers
The characteristics of bead welding on steel with process parameter during the laser-arc hybrid welding(Ⅰ) - Effect of flow rate of shield gas and distance between laser and arc -
- Jong-Do Kim, Gi-Hoon Myung, Moo-Keun Song, Jae-Hwan Oh, Jeong Suh
- J Weld Join. 2015;33(2):85-90.
-
A Study of Weldability for Pure Titanium by Nd:YAG Laser(Ⅲ) - Weld Properties of Edge Welding
- Jong-Do Kim, Byung-Lea Kil, Myung-Sub Kwak, Moo-Keun Song
- Journal of KWJS. 2009;27(6):74-79.
-
A Study of Weldability for Pure Titanium by Nd:YAG Laser(Ⅱ) - Welding Properties of Butt Welding
- Jong-Do Kim, Myung-Sub Kwak, Moo-Keun Song, Seung-Ha Park
- Journal of KWJS. 2009;27(6):68-73.