A Study on Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW
Jun Hyeok Hyun, Tae Woo Shin, Sang Ho Kim, Jin Hyun Koh
J Weld Join. 2017;35(4):74-81.