Research Papers
A Study on Mechanical Properties of Austenitic Stainless Steel Welds Using ArcTig Welding
Sung-Hyun Jeon, Tae-Wan Kim, Woo-Hyeon Ju, Yu-Chan Kim
J Weld Join. 2022;40(4):343-351.
Research Papers
Study on the Improvement of TIG Welding Productivity through Analysis of ArcTig Welding Properties
Sung-Hyun Jeon, Tae-Wan Kim, Young-Woong Lee, Yu-Chan Kim