Research Papers Optimization of Friction Stir Welding Parameters of AA2014-T6 Alloy using Taguchi Statistical Approach
Wali Muhammad, Wilayat Husain, Anjum Tauqir, Abdul Wadood
J Weld Join. 2020;38(5):493-501.