Journal of KWJS. 2012;30(2):16-21. Published online May 16, 2012.
DOI: https://doi.org/10.5781/KWJS.2012.30.2.16
The Study of Measurement of Residual Stress for Pipe Weldments of Power Plant
Sang-Ki Park, Yean-Shik Ahn, Doo-Song Gil