Journal of KWJS. 2013;31(4):42-46. Published online August 31, 2013.
DOI: https://doi.org/10.5781/KWJS.2013.31.4.42
- Wear Resistance Evaluation of Contact Tip according to Flux Cored Wire
-
Dong-yoon Kim1, In-Sung Hwang1, Dong-Cheol Kim1, Moon-Jin Kang1
-
- Corresponding author: In-Sung Hwang ,Email: hisman@kitech.re.kr
- Abstract
- The contact tip for flux cored arc welding has important functions to transmit the welding current to the wire and to guide the wire to molten pool. A damaged contact tip causes a productivity reduction and a welding quality problem. In this study, the welding experiments for the wear resistance of contact tip regarding flux cored wire types were performed. With two fold type and a seamless type flux cored wires, the wear rates of contact tips were compared. In addition, the wear rate was checked according to the contact tip position.
Keywords :Wear resistance, Contact tip, Flux cored wire, Wear rate, Fold type, Seamless type