Journal of KWJS. 1986;4(2):21-29. Published online June 25, 1986.
- The Effect of Welding Heat Input and Heat-Treatment on the Strength of the Electron Beam Welded 175kg/mm² Maraging Steel Sheet
-
윤한상, 정병호, 배차헌
-