Journal of KWJS. 1993;11(2):74-85. Published online June 25, 1993.
- Formation of Thicker hard Alloy Layer on Aluminum Alloy by PTA Overlaying with Metal Powders - Effect of Si Adding on Hardening Characteristics and Wear Resistance of Alloyed Surface Layer -
-
박성두, 이영호, 中田一博, 松田福久
-