Journal of KWJS. 1994;12(4):63-75. Published online December 26, 1994.
- A Study on the Stress Corrosion Cracking Evaluation for Weld Joint of Steel by Using Miniaturized Small Specimen
-
유효선, 임재규, 정세희
-