Journal of KWJS. 1995;13(2):139-149. Published online June 26, 1995.
- Evaluation of Underclad Crack Susceptibility of the SA508 Class 3 Steel for Pressure Vessels - Optimization of Heat Input -
-
김석원, 양성호, 김준구, 이영호
-