Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88
Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89
-
-
Journal of KWJS. 1996;14(3):66-74. Published online June 25, 1996.
- A Study on the Evaluation of the Friction and Wear Properties of the Sprayed Coating Layer
-
김영식, 김윤해, 김종호, 최영국, 강태영
-