Journal of KWJS. 1998;16(5):108-118. Published online October 26, 1998.
- Construction of Chaos simulator for Ultrasonic Pattern Recognition Evaluation of Weld Zone in Austenitic Stainless Steel 304
-
이원, 윤인식, 장영권
-