Journal of KWJS. 2000;18(6):48-54. Published online December 25, 2000.
- Effect of Heat Treatment on the Microstructures and Properties of HVOF Sprayed Ni-Cr-W-Mo-B Alloy Coatings
-
민경오, 이창희
-