Journal of KWJS. 2002;20(1):62-68. Published online February 25, 2002.
- A Study of the Infrared Temperature Sensing System for Surface Temperature Measurement in Laser Welding(Ⅰ)-Surface Temperature Profile According to Read Shape-
-
이목영, 김재웅
-