Journal of KWJS. 2002;20(2):65-70. Published online April 25, 2002.
- A Study on the GMA Welding Characteristics of Al5083-O Aluminum Alloy According to the Shield Gas Mixing Ratio and Heat Input
-
정재강, 양훈승, 이동길
-