Journal of KWJS. 2002;20(3):98-104. Published online June 25, 2002.
- Microstructural Characteristics of Zircaloy-4 Nuclear Fuel Cladding Welds by Resistance Upset Welding Processes
-
고진현, 김상호, 박춘호, 김수성
-