Journal of KWJS. 2006;24(1):77-87. Published online April 3, 2006.
- [Research Papers] Prediction Model for the Microstructure and Properties in Weld Heat Affected Zone : Ⅱ. Prediction Model for the Austenitization Kinetics and Austenite Grain Size Considering the Effect of Ferrite Grain Size in Fe - C - Mn Steel
-
Jong-Geun Ryu, Joon-Oh Moon, Chang-Hee Lee, Sang-Ho Uhm, Jong-Bong Lee, Woong-Sung Chang
-
- Abstract
- Considering ferrite grain size in the base metal, the prediction model for Ac₃ temperature and prior austenite grain size at just above Ac₃ temperature was proposed. In order to predict Ac₃ temperature, the Avrami equation was modified with the variation of ferrite grain size, and its kinetic parameters were measured from non-isothermal data during continuous heating. From calculation using a proposed model, Ac₃ temperatures increased with increasing ferrite grain size and heating rate. Meanwhile, by converting the phase transformation kinetic model that predicts the ferrite grain size from austenite grain size during cooling, a prediction model for prior austenite grain size at just above the Ac₃ temperature during heating was developed.